Ensinger Sintimid™ V 40% graphite Polyimide (PI)  (discontinued **)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Graphite Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Sintimid™ V 40% graphite Polyimide (PI)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V is characterized by its long-term thermal stability, outstanding wear resistance, high creep resistance, and strength up to its continuous use temperature of 572°F. Specialty grades containing internal lubricants such as graphite are available for applications requiring improved wear resistance and lower coefficients of friction.Superior high temperature characteristicsExcellent long-term thermal stabilityOutstanding bearing and wear properties (at elevated temperatures, SINTIMID™ V formulations offer superior wear rates)Excellent creep resistanceHigh strength and stiffness properties (SINTIMID™ V has a tensile strength of 20,000 psi at room temperature)High purity characteristics (only extremely low levels of extractables and ionic impurities are apparent in SINTIMID™ V)Good chemical resistance (SINTIMID™ V is not attacked by common solvents or fuels and is acceptable for use in contact with many acids)SINTIMID™ V with its superior physical properties, is ideal for applications in the aerospace, nuclear, automotive, electrical/electronic, and chemical processing industries. It is an excellent candidate for high purity applications in the semiconductor processing industry. Typical components produced from SINTIMID™ V include seals, thrust washers, bushings and wear pads in transportation/off-highway equipment, insulating and support elements in electrical welding and brazing equipment, and wafer-handling components in the harsh environment of semiconductor plasma ovens. Pump and valve seals, vanes, and piston rings are also commonly produced from SINTIMID™ V.Information Provided by Ensinger Industries, Inc.Sintimid has been replaced with Tecasint in the Ensinger product line.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
ASTM D792
Density 1.56 g/cc
0.0563 lb/in³
ASTM D792
Water Absorption 0.87 %

@Temperature 22.8 °C,
Time 86400 sec
0.87 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 111
111
ASTM D785
Tensile Strength, Yield 64.8 MPa

@Temperature 22.8 °C
9400 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 2.2 %

@Temperature 22.8 °C
2.2 %

@Temperature 73.0 °F
ASTM D638
Flexural Strength 100 MPa

@Temperature 22.8 °C
14500 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 4.00 GPa

@Temperature 22.8 °C
580 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.160 J/cm

@Temperature 22.8 °C
0.300 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Maximum Service Temperature, Air 280 °C
536 °F
Long Term
330 °C
626 °F
Intermittent
Deflection Temperature at 1.8 MPa (264 psi) >= 316 °C
>= 600 °F
ASTM D648