Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECAPET™ PET Polyethylene Terephthalate (PET)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Ensinger
Trade Name TECAPET™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECAPET™ PET Polyethylene Terephthalate (PET).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and superior dimensional stability make it a versatile material for designing mechanical and electro-mechanical parts. Because TECAPET™ PET has no centerline porosity, the possibility of fluid absorption and leakage is virtually eliminatedExcellent wear resistanceLow coefficient of frictionVery good chemical resistanceNo centerline porosity eliminates the possibility of fluid absorption and leakageGood electrical insulatorHigh mechanical strengthExcellent hardness and stiffnessGood weather resistanceIn compliance with FDA regulations 21 CFR 177.1630 for use in contact with foodLow water absorptionGood resistance to high-energy radiationTECAPET™ PET superior wear resistance and lack of centerline porosity give it an advantage over other materials for applications involving solvents, chemicals, and food products. TECAPET™ PET is also used in water purification systems, printing equipment, textile components, food-handling equipment, and valves.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.10 %

@Temperature 22.8 °C,
Time 86400 sec
0.10 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.50 %

@Temperature 22.8 °C
0.50 %

@Temperature 73.0 °F
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength, Yield 86.2 MPa

@Temperature 22.8 °C
12500 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 20 %

@Temperature 22.8 °C
20 %

@Temperature 73.0 °F
ASTM D638
Tensile Modulus 3.24 GPa
470 ksi
ASTM D638
Flexural Strength 121 MPa

@Temperature 22.8 °C
17600 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 2.96 GPa

@Temperature 22.8 °C
430 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature 22.8 °C
0.700 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Coefficient of Friction, Dynamic 0.25

@Pressure 0.276 MPa
0.25

@Pressure 40.0 psi
50 fpm; ASTM D3702
Coefficient of Friction, Static 0.19
0.19
ASTM D3702
K Factor (Wear Factor) 2.1e-8

@Pressure 0.276 MPa
2.1e-8

@Pressure 40.0 psi
(in<sup>3</sup>/hr)x(1/PV), 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 70.2 µm/m-°C
39.0 µin/in-°F
ASTM D696
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
UL746B
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
Melting Point 254 °C
490 °F
ASTM D3418
Maximum Service Temperature, Air 110 °C
230 °F
Long Term
160 °C
320 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 60.0 Hz,
Temperature 22.8 °C
3.4

@Frequency 60.0 Hz,
Temperature 73.0 °F
50% RH; ASTM D150
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 60.0 Hz,
Temperature 22.8 °C
0.0020

@Frequency 60.0 Hz,
Temperature 73.0 °F
ASTM D150
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved