Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ensinger
Trade Name TECAPRO™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAPRO™ MT is an FDA approved homopolymer polypropylene based material with exceptionally low residual stress to facilitate the fabrication of dimensionally stable parts with varying cross sections.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 35.00 MPa
5076 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Unnotched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
ASTM D648
Users viewing this material also viewed the following: