Ensinger TECASON™ P Polyphenylsulfone (PPSU)

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Ensinger
Trade Name TECASON™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECASON™ P Polyphenylsulfone (PPSU).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties.
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Yield 69.6 MPa
10100 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Flexural Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Compressive Strength 98.94 MPa
14350 psi
ASTM D695
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Maximum Service Temperature, Air 182 °C
360 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
420 °F
ASTM D648
Vicat Softening Point 218 °C
424 °F
ASTM D1525
Flammability, UL94 V-0
V-0
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.44

@Frequency 60.0 Hz
3.44

@Frequency 60.0 Hz
50% RH; ASTM D150
Dielectric Strength 14.2 kV/mm
360 kV/in
ASTM D149