Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ensinger
Trade Name Tecamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tecamid® 6/6 GF30 is a 30% glass-fiber reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection temperature, and superior abrasion and wear resistance. While all Tecamid® materials have high mechanical strength and superior resistance to wear and organic chemicals, Tecamid® 6/6 GF30 has more than double the strength and stiffness of unreinforced nylons and a heat deflection temperature which approaches its melting point. Superior organic chemical resistance High heat deflection temperature Excellent wear resistance High strength and stiffness Very good fatigue endurance Superior creep resistance Tecamid® 6/6 GF30 has an excellent balance of properties which make it an ideal material for metal replacement in applications such as automotive parts, industrial valves, railway tie insulators, and other industry uses whose design requirements include high strength, toughness, and weight reduction.Information provided by Ensinger Inc.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
at 24 hours; ASTM D570
Water Absorption at Saturation 5.4 %
5.4 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D785
Tensile Strength, Yield 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 128 MPa
18500 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.6 µm/m-°C

@Temperature 20.0 °C
12.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D2133
Maximum Service Temperature, Air 110 °C
230 °F
Long Term; ASTM UL746B
241 °C
465 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
490 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM D648