Material Notes:
Tecapeek™ ID metal detectable polyetheretherketone, made from Victrex® PEEK 450G polymer, is formulated to reduce the risk of product contamination and allow for easy detection of fragments in the unlikely event of failure.Typical applications for TECAPEEK™ ID are highly stressed parts such as high temperature kettle scrapers and agitators.Information provided by Ensinger Inc.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 4.5 %
4.5 %
ISO 527
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ASTM D638
Flexural Modulus 4.40 GPa
638 ksi
ASTM D790
Charpy Impact, Notched 4.50 J/cm²
21.4 ft-lb/in²
ISO 178
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DIN 53 765
Maximum Service Temperature, Air 260 °C
500 °F
Long Term
300 °C
572 °F
Short Term
Glass Transition Temp, Tg 143 °C
289 °F
DIN 53 765
Flammability, UL94 V-0
V-0