Ensinger Tecapeek® MT Polyetheretherketone (PEEK)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Ensinger
Trade Name Tecapeek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® MT Polyetheretherketone (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties allow engineers and designers the ability to create cost-effective, innovative parts that exhibit outstanding wear, heat, electrical and chemical resistance. The TECAPEEK™ family is made up of materials for medical applications.TECAPEEK™ MT, unfilled pigmented medical grade PEEK™TECAPEEK™ XP98, compression molded 30% carbon fiber filled PEEK (isotropic properties)TECAPEEK™ MT CF30, extruded 30% carbon fiber filled PEEKTECAPEEK™ Classic™, ISO 10993 certification by resin and extrusion lot of 30 days contactTECAPEEK™ Classix™ XRO-20 radio opaque grade with 20% BaSO4 addedThe TECAPEEK™ family of high performance plastics are high effective in the creation and manufacture of high quality medical instruments. Five separate grades, each with qualities to meet a wide range of requirements for the engineer and product designer.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Water Absorption at Saturation 0.10 %

@Temperature 22.8 °C,
Time 86400 sec
0.10 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 99
99
ASTM D785
Tensile Strength, Yield 94.975 MPa

@Temperature 22.8 °C
13775 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 3.00 GPa

@Temperature 22.8 °C
435 ksi

@Temperature 73.0 °F
1% Secant; ASTM D638
Flexural Strength 186 MPa

@Temperature 22.8 °C
27000 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 4.10 GPa

@Temperature 22.8 °C
595 ksi

@Temperature 73.0 °F
ASTM D790
Compressive Strength 117 MPa

@Temperature 22.8 °C
16900 psi

@Temperature 73.0 °F
ASTM D695
Shear Strength 51.7 MPa

@Temperature 22.8 °C
7500 psi

@Temperature 73.0 °F
Ultimate; ASTM D3846
Izod Impact, Notched 0.641 J/cm

@Temperature 22.8 °C
1.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 46.8 µm/m-°C
26.0 µin/in-°F
ASTM D696
Melting Point 340 °C
644 °F
Maximum Service Temperature, Air 260 °C
500 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D149
Surface Resistivity per Square 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Strength 7.87 kV/mm
200 kV/in
ASTM D257