Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-91 Compression Molded PEEK Compound, 30% Fiberglass

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-91 Compression Molded PEEK Compound, 30% Fiberglass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Typical Applications:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Filler Content 30 %
30 %
Crystallinity 30 %
30 %
Mechanical Properties Metric English Comments
Hardness, Shore D 91
91
ASTM D2240
Tensile Strength 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.395 J/cm
0.740 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Tan