Material Notes:
Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 88.3 MPa
12800 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.934 J/cm
1.75 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.14
0.14
Coefficient of Friction, Static 0.16
0.16
ASTM D3702
K (wear) Factor 98.7 x 10-8 mm³/N-M
49.0 x 10-10 in³-min/ft-lb-hr
ASTM D3702
Limiting Pressure Velocity 0.560 - 0.596 MPa-m/sec
16000 - 17000 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear 72.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
40.0 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 93.3 °C
200 °F
Continuous
166 °C
330 °F
Intermittent
Copyright © lookpolymers.com All Rights Reserved