Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 120
120
ASTM D785
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength 27.6 MPa
4000 psi
ASTM D638
Elongation at Break 0.30 %
0.30 %
ASTM D638
0.40 %
0.40 %
Flexural Strain; ASTM D790
Tensile Modulus 9.65 GPa
1400 ksi
ASTM D638
Flexural Strength 53.1 MPa
7700 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Compressive Strength <= 152 MPa
<= 22000 psi
ASTM D695
Shear Strength 40.0 MPa
5800 psi
ASTM D732
Izod Impact, Notched 0.347 J/cm
0.650 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.11
0.11
ASTM D1894
Coefficient of Friction, Static 0.14
0.14
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 19.3 µm/m-°C
10.7 µin/in-°F
ASTM E831
Maximum Service Temperature, Air 232 °C
450 °F
UL746B
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black