Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Carbon Fiber
Manufacturer Ensinger
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability and creep resistance.The XP 130 Series of Polyimide is a non-melting high temperature thermoplastic with high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance along with good chemical resistance.Applications:Thermal & electrical insulatorsSwitch PartsVacuum SealsPlug PartsChip CarriersHot glass gripper fingersBalls for control valvesHousing PartsWelding EquipmentInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Tensile Strength 36.5 MPa
5300 psi
ASTM D638
Elongation at Break 0.80 %
0.80 %
ASTM D638
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Flexural Strength 97.9 MPa
14200 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Compressive Strength <= 194 MPa
<= 28200 psi
ASTM D695
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved