Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Entec Engineered Resins
Trade Name Hylox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hylox® 9230BK PBT, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
Flexural Strength 169 MPa
24500 psi
ASTM D790
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Izod Impact, Notched 0.796 J/cm
1.49 ft-lb/in
73°F; ASTM D256
Processing Properties Metric English Comments
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Front Barrel Temperature 243 - 254 °C
470 - 490 °F
Nozzle Temperature 243 - 254 °C
470 - 490 °F
Melt Temperature 249 - 260 °C
480 - 500 °F
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Drying Temperature 121 °C
250 °F
Dry Time <= 12 hour
<= 12 hour
Moisture Content <= 0.020 %
<= 0.020 %
Injection Pressure 6.89 - 11.7 MPa
1000 - 1700 psi
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Shot Size 40 - 80 %
40 - 80 %
Screw Speed 40 - 80 rpm
40 - 80 rpm
Descriptive Properties Value Comments
Holding Pressure 500 to 900 psi
Injection Rate Moderate-Fast