Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypel® PEHD18/.956 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Entec Engineered Resins
Trade Name Hypel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypel® PEHD18/.956 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Yield 7.7 %
7.7 %
ASTM D638
Flexural Modulus 1.15 GPa
167 ksi
2% Secant; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
Unannealed (0.250 in); ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Users viewing this material also viewed the following: