Entec Hyril® SAN500 Styrene Acrylonitrile

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent
Manufacturer Entec Engineered Resins
Trade Name Hyril®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hyril® SAN500 Styrene Acrylonitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Features: Copolymer Form: PelletsInformation provided by Entec
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength, Yield 71.7 MPa
10400 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 123 MPa
17900 psi
ASTM D790
Flexural Modulus 3.87 GPa
561 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.4 µm/m-°C
33.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM D648
Vicat Softening Point 108 °C
227 °F
Rate B (120°C/h), Loading 1 (10 N); ASTM D1525
Optical Properties Metric English Comments
Haze 0.60 %
0.60 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Users viewing this material also viewed the following: