Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Enviro Tech International EnSolv® 5408 n-Propyl Bromide Vapor Degreasing Solvent

Category Fluid , Solvent
Manufacturer Enviro Tech International, Inc.
Trade Name EnSolv®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Enviro Tech International EnSolv® 5408 n-Propyl Bromide Vapor Degreasing Solvent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EnSolv-5408 is the only Boeing approved, stabilized n-Propyl Bromide based solvent for the replacement of Trichloroethylene, Perchloroethylene and 1,1,1-trichloroethane in aerospace vapor degreasing. EnSolv-5408 is listed as an approved material on Boeing’s BMS 11-11 specification for use under BAC 5408. In addition, EnSolv-5408 has been approved by Bell Helicopter under Materials Bulletin 1918 for vapor degreasing. EnSolv-5408 is a patented azeotropic mixture that can be distilled and reused through numerous cycles before it needs to be replaced. EnSolv-5408 is compatible with all metals and many plastics and other materials typically cleaned in vapor degreasers. EnSolv-5408 has passed all stress corrosion and hydrogen embrittlement tests for titanium. Information provided by Enviro Tech International.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
75°F (water = 1)
Density 0.00512 g/cc
0.000185 lb/in³
Vapor Density
Water Absorption <= 0.010 %
<= 0.010 %
Vapor Pressure 0.179 bar

@Temperature 25.0 °C
134 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.09 J/g-°C
0.260 BTU/lb-°F
Boiling Point 70.0 °C
158 °F
Flammability Test 3.8 - 9.5
3.8 - 9.5
vol% limits based on n-Propyl Bromide
Electrical Properties Metric English Comments
Dielectric Breakdown 21000 V
21000 V
AC
Descriptive Properties Value Comments
Acid Acceptance, as NaOH >0.19% by wt.
Acidity , as HCl < 0.0010% by wt.
Appearance Clear; free of suspended matter
Base Materials Meets ASTM D6368 Yes
Evaporation Rate (Butyl Acetate = 1) 4.7
Flash Point TCC None
Kauri Butanol Number 130
Users viewing this material also viewed the following: