Material Notes:
Material Description: A two component, high Tg, high temperature grade epoxy designed for semiconductor, underfill, hard-disk drive and hybrid micro-electronics packaging applications. The epoxy can also be used for adhesive and sealing applications in electronics, optical, and medical devices.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
1.12 g/cc
1.12 g/cc
Part A
Viscosity 45000 - 70000 cP

@Temperature 23.0 °C
45000 - 70000 cP

@Temperature 73.4 °F
50 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Tensile Modulus 1.68 GPa
244 ksi
Storage
Shear Strength >= 13.8 MPa
>= 2000 psi
Lap
>= 23.4 MPa
>= 3400 psi
Die
Thermal Properties Metric English Comments
CTE, linear 43.0 µm/m-°C
23.9 µin/in-°F
Below Tg
165 µm/m-°C
91.7 µin/in-°F
Above Tg
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
350 °C
662 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 100 °C
>= 212 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 468 °C
874 °F
Degradation Temperature
Optical Properties Metric English Comments
Refractive Index 1.5657

@Wavelength 589 nm
1.5657

@Wavelength 589 nm
Transmission, Visible 88 %

@Wavelength 800 nm
88 %

@Wavelength 800 nm
Spectral
>= 94 %

@Wavelength 880 - 1600 nm
>= 94 %

@Wavelength 880 - 1600 nm
Spectral
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
Dielectric Constant 3.08

@Frequency 1000 Hz
3.08

@Frequency 1000 Hz
Dissipation Factor 0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 150 °C
0.0167 hour

@Temperature 302 °F
minimum
30.0 min

@Temperature 80.0 °C
0.500 hour

@Temperature 176 °F
minimum
Pot Life 180 min
180 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Part B
White
Part A
Consistency Pourable paste
Mix Ratio By Weight 10:1
Number of Components Two
Weight Loss 0.38%
200°C
0.5%
250°C
0.84%
300°C
Users viewing this material also viewed the following: