Material Notes:
Material Description: A single component, low viscosity, UV curable adhesive designed for curing in seconds. It is an all-purpose, general adhesive for optical applications including fiber optic components, DVD, medical, and PCB level electro-optics. It can also be used for sealing and coating applications. It meets the requirements of USP Class VI biocompatibility standards for medical implants.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Viscosity 150 - 250 cP

@Temperature 23.0 °C
150 - 250 cP

@Temperature 73.4 °F
100 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Tensile Modulus 1.73 GPa
251 ksi
Storage
Shear Strength >= 7.03 MPa
>= 1020 psi
Die
Thermal Properties Metric English Comments
CTE, linear 69.0 µm/m-°C
38.3 µin/in-°F
Below Tg
170 µm/m-°C
94.4 µin/in-°F
Above Tg
Maximum Service Temperature, Air 200 °C
392 °F
Continuous
300 °C
572 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 70.0 °C
>= 158 °F
Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Decomposition Temperature 385 °C
725 °F
Degradation Temperature
Optical Properties Metric English Comments
Refractive Index 1.4736

@Wavelength 589 nm
1.4736

@Wavelength 589 nm
Transmission, Visible >= 98 %

@Wavelength 420 - 1600 nm
>= 98 %

@Wavelength 420 - 1600 nm
Spectral
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear/Colorless
before cure
Consistency Pourable liquid
Number of Components Single
Weight Loss 0.79%
200°C
1.2%
250°C
1.9%