Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer Epoxyset
Trade Name Epoxiohm
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by elevated temperatures.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
Viscosity 1000 - 1600 cP
1000 - 1600 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D2240
Shear Strength 12.0 MPa
1740 psi
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 62.0 µm/m-°C
34.4 µin/in-°F
Thermal Conductivity 1.60 W/m-K
11.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 65.0 °C
149 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000500 ohm-cm
0.000500 ohm-cm
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 80.0 °C
3.00 hour

@Temperature 176 °F
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Pot Life 240 min
240 min