Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Esstech V-116-1130 Barium Silicate Glass

Category Ceramic , Glass , Glass Ceramic
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech V-116-1130 Barium Silicate Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Barium Silicate glass is an inorganic filler with a high refractive index of 1.580. It also has a high coefficient of thermal expansion and a high barium content, which increases its x-ray opacity. CAS # 65997-17-3.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Particle Size 13 µm
13 µm
median
Thermal Properties Metric English Comments
CTE, linear 6.70 µm/m-°C
3.72 µin/in-°F
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
Component Elements Properties Metric English Comments
BaO 46 %
46 %
SiO2 49 %
49 %
Users viewing this material also viewed the following: