Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Esstech X-127-0950 Poly Methyl Methacrylate

Category Polymer , Thermoset , Methacrylate
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-127-0950 Poly Methyl Methacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Our polymethyl methacrylate, PMMA is manufactured "plasticizer-free" with a molecular weight range of 925000 to 975000. No extraneous material detected. CAS # 9011-14-7.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Molecular Weight 925000 - 975000 g/mol
925000 - 975000 g/mol
Users viewing this material also viewed the following: