Esstech X-887-7446 1,6-Hexanediol Dimethacrylate, C14H22O4

Category Polymer , Thermoset , Methacrylate
Manufacturer Esstech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-887-7446 1,6-Hexanediol Dimethacrylate, C14H22O4.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Toxic Substance Control Act List. CAS # 6606-59-3.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.996 g/cc
0.996 g/cc
Molecular Weight 254.326 g/mol
254.326 g/mol
Optical Properties Metric English Comments
Refractive Index 1.455
1.455
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Acidity (% Methacrylic Acid) < 0.1
Color (APHA) < 75
MeHQ Inhibitor (ppm) 80-120
Purity (%) > 95