Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Evacell EVA 100 EVA + PE Foam

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Polyethylene (PE)
Manufacturer Eurofoam s.r.l.
Trade Name Evacell
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Evacell EVA 100 EVA + PE Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, dielectric properties and good insulating properties. It is resistant to UVA radiation. It can be silk-screened and thermoformed.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.0800 - 0.100 g/cc
0.00289 - 0.00361 lb/in³
ISO 845-88
Water Absorption <= 3.0 %
<= 3.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 70 - 80
70 - 80
ASTM D 2240
Tensile Strength 1.30 MPa
189 psi
ASTM D 412
Elongation at Break >= 130 %
>= 130 %
ASTM D 412
Compressive Yield Strength 0.0900 MPa

@Strain 25.0 %
13.1 psi

@Strain 25.0 %
ASTM 1056/85
Tear Strength 0.330 kN/m
1.88 pli
ASTM D 624
Compression Set 10 %

@Strain 25.0 %
10 %

@Strain 25.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
ASTM D 3575
Minimum Service Temperature, Air -10.0 °C
14.0 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Closed
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Users viewing this material also viewed the following: