Physical Properties Metric English Comments
Density 0.0400 - 0.0500 g/cc
0.00145 - 0.00181 lb/in³
ISO 845-88
Water Absorption 0.30 %
0.30 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 57 - 67
57 - 67
ASTM D 2240
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Elongation at Break >= 150 %
>= 150 %
ASTM D 412
Compressive Yield Strength 0.0500 MPa

@Strain 25.0 %
7.25 psi

@Strain 25.0 %
ASTM 1056/85
Tear Strength 0.640 kN/m
3.65 pli
ASTM D 624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
ASTM D 3575
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
ASTM D 3575
Shrinkage <= 8.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 8.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black, White
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC