Eurostar Star L POM D51 POM, Injection Molded

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Eurostar Engineering Plastics
Trade Name Star L
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Star L POM D51 POM, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.022 - 0.024 cm/cm

@Thickness 4.00 mm
0.022 - 0.024 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Elongation at Break 13 %
13 %
ISO 527
Flexural Strength 64.0 MPa
9280 psi
ISO 178
Flexural Modulus 2.05 GPa
297 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 33.0 kJ/m²
15.7 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Be
Processing Properties Metric English Comments
Zone 1 180 - 190 °C
356 - 374 °F
Zone 2 180 - 190 °C
356 - 374 °F
Zone 3 180 - 200 °C
356 - 392 °F
Melt Temperature 180 - 200 °C
356 - 392 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.10 %
0.10 %