Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Eurostar Engineering Plastics
Trade Name Starflam
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Staramide RX06082 is a Halogen Free and Red Phosphorous Free, flame Retardant, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 4.00 mm
0.0030 - 0.0050 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 111 MPa
16100 psi
5 mm/min; ISO 527
Elongation at Break 2.6 %
2.6 %
5 mm/min; ISO 527
Flexural Yield Strength 161 MPa
23400 psi
2 mm/min; ISO 178
Flexural Modulus 7.00 GPa
1020 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80x10x4; ISO 179/1eA
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Zone 1 260 - 270 °C
500 - 518 °F
Zone 2 265 - 280 °C
509 - 536 °F
Zone 3 260 - 280 °C
500 - 536 °F
Melt Temperature 265 - 275 °C
509 - 527 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.20 %
0.20 %