Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen HU 30E4 ECR is a reinforced Polypropylene with a low carbon footprint renewable mineral filler, Injection Molding Resin (also known as HUS30E4ECR)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm

@Thickness 4.00 mm
0.018 - 0.020 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ISO 527
Elongation at Break 8.0 %
8.0 %
ISO 527
Flexural Strength 41.0 MPa
5950 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 190 - 200 °C
374 - 392 °F
Zone 2 190 - 200 °C
374 - 392 °F
Zone 3 190 - 200 °C
374 - 392 °F
Melt Temperature 190 - 200 °C
374 - 392 °F
Mold Temperature 35.0 - 50.0 °C
95.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour