Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Filler Content 15 %
15 %
ISO 3451
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 7.5 %
7.5 %
23°C; ISO 62
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 527
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
12.5 J/cm²

@Temperature 23.0 °C
59.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-1/2
Vicat Softening Point 240 °C
464 °F
50N; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 500 V
500 V
IEC 60112
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved