Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Exxon Chemical
Trade Name ACHIEVE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A homopolymer resin based on Exxpol™ metallocene technology designed for medical, electronics and other applications requiring cleanliness. It provides lower, volatiles and extractables and better clarity than convention homopolymersAvailability: North America Features: Autoclave SterilizableEthylene Oxide SterilizableGood Organoleptic PropertiesLow EmissionsLow ExtractablesSteam SterilizableApplications: Automotive ApplicationsIndustrial ApplicationsLabwareMedical PackagingMedical/Healthcare ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
Melt Flow 32 g/10 min

@Load 2.16 kg,
Temperature 230 °C
32 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
2 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
1% secant, 0.05 in/min.; ASTM D790A
Izod Impact, Notched 0.176 J/cm
0.330 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 149 °C
300 °F
DSC Melting Temp.; ExxonMobil Method
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648