Material Notes:
Product Description: ExxonMobil EN 33900 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesApplications: Hot Melt AdhesivesHot Melt SealantsWax Blends Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ExxonMobil method
Viscosity 8300 cP

@Temperature 190 °C
8300 cP

@Temperature 374 °F
ASTM D3236
Butyl Acrylate Content 32.5 %
32.5 %
ExxonMobil Method
Melt Flow 900 g/10 min

@Load 2.16 kg,
Temperature 190 °C
900 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 44

@Time 15.0 sec
44

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 0.965 MPa
140 psi
ASTM D638
Elongation at Break 140 %
140 %
ASTM D638
Flexural Modulus, 1% Secant 5.38 MPa
780 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 140 °C
<= 284 °F
Peak Melting Point; ExxonMobil method