ExxonMobil Escor™ 5070 Ethylene Acrylic Acid Copolymer Resin

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Exxon Chemical
Trade Name Escor™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escor™ 5070 Ethylene Acrylic Acid Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Escor 5070 is an ethylene acrylic acid copolymer characterized by high melt index and 9% acrylic acid comonomer content. Escor 5070 combines easily processing and adhesion to polar materials, it can be formulated and UV-stabilized for use in outdoor applications.Availability: Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Adhesive ApplicationsHeat Seal LayerMasterbatch Base ResinPowder Coating to Polar Substrates Information provided by ExxonMobil
Physical Properties Metric English Comments
Acrylic Acid Content 9.0 %
9.0 %
ExxonMobil Method
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Thermal Properties Metric English Comments
Melting Point <= 203 °C
<= 397 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 73.9 °C
165 °F
ASTM D1525