ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Exxon Chemical
Trade Name Escor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at high line speed. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and glass. Offers excellent balance of adhesion onto the substrates and interlayer adhesion with coextruded LDPE and EVA’s.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Aluminum Containing PackagingCoextrusion Coating Cosmetic Packaging Extrusion CoatingExtrusion LaminationFood packaging Hygiene PackagingMetalized Films Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ExxonMobil method
Acrylic Acid Content 6.0 %
6.0 %
ExxonMobil Method
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 5.08 cm

@Temperature 280 °C
2.00 in

@Temperature 536 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
6.86 cm

@Temperature 280 °C
2.70 in

@Temperature 536 °F
164 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 3.50 m/s
689 ft/min
Constant output at 35 rpm; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point <= 216 °C
<= 421 °F
Peak Melting Point; ExxonMobil method