ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification  (discontinued **)

Category Polymer , Thermoplastic , EMAAA Terpolymer , Ethylene Methyl Acrylate
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, etc.Applications: Low temperature sealant; Engineering thermoplastic modifier; Heat activated sealant; Adhesive for polyolefins to metals or polar polymers.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
Exxon Method
Melt Flow 5.0 g/10 min
5.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Hardness, Shore D 34
34
ASTM D2240
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 660 %
660 %
ASTM D638
Modulus of Elasticity 0.00860 GPa
1.25 ksi
ASTM D638
Flexural Modulus 0.0190 GPa
2.76 ksi
ASTM D790
Tensile Impact Strength 760 kJ/m²
362 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 76.0 °C
169 °F
Exxon Method
Vicat Softening Point 43.0 °C
109 °F
1000g; ASTM D-1525
Glass Transition Temp, Tg 56.0 °C
133 °F
DSC