ExxonMobil Escorene™ AD 2528EH2 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ AD 2528EH2 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: AD 2528EH2 is a copolymer of ethylene and vinyl acetate. Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: Yes Applications:Hot Melts AdhesivesViscosity Modifier Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil method
Viscosity 3200 cP

@Temperature 190 °C
3200 cP

@Temperature 374 °F
Melt
Vinyl Acetate Content 27.5 %
27.5 %
ExxonMobil method
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.93 MPa
280 psi
Molded Properties; ASTM D638
Elongation at Break 160 %
160 %
Molded Properties; ASTM D638
Tensile Modulus 0.0138 GPa
2.00 ksi
Molded Properties; ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 158 °C
<= 316 °F
Peak Melting Point; ExxonMobil method