Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD-720 High EVA Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-720 High EVA Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength properties and toughness. This resin is also used in specialized molding applications.Applications: Coextruded heat seal layer in food packaging film; Shoe soles (injection molded).
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 1.5 g/10 min
1.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
ASTM D2240
Hardness, Shore D 30
30
ASTM D2240
Tensile Strength, Ultimate 13.0 MPa
1890 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0530 GPa
7.69 ksi
1% Secant, ASTM D790
Tensile Impact Strength 627 kJ/m²
298 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
Exxon Method
Vicat Softening Point 64.0 °C
147 °F
1000g; ASTM D-1525
Copyright © lookpolymers.com All Rights Reserved