Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excellent sealing material with a very low seal initiation temperature and high clarity.Availability: Latin America, North America and South America Applications:Adhesive LaminationBarrier Food PackagingCoextrusion CoatingCompoundingDocument PlastificationExtrusion CoatingExtrusion LaminationFlexible PackagingHigh Frequency SealingIndustrial PackagingInjection MoldingMasterbatch Base ResinNon-woven CoatingPVC ReplacementThermal LaminationWire and Cable CompoundsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ExxonMobil method
Vinyl Acetate Content 18 %
18 %
ExxonMobil method
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 190 °C
14 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 9.40 cm

@Temperature 230 °C
3.70 in

@Temperature 446 °F
656 ft/min, constant output at 35 rpm; ExxonMobil Method
10.9 cm

@Temperature 230 °C
4.30 in

@Temperature 446 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 9.00 m/s

@Temperature 230 °C
1770 ft/min

@Temperature 446 °F
Constant output at 35 rpm; ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A >= 90

@Time 15.0 sec
>= 90

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 34

@Time 15.0 sec
34

@Time 0.00417 hour
ASTM D2240
Film Elongation at Break, MD >= 800 %
>= 800 %
ASTM D882
Film Tensile Strength at Break, MD 7.58 MPa
1100 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 181 °C
<= 358 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Users viewing this material also viewed the following: