Material Notes:
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 0.70 g/10 min
0.70 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Hardness, Shore D 39
39
ASTM D2240
Tensile Strength, Ultimate 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 5.00 MPa
725 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0520 GPa
7.54 ksi
1% Secant, ASTM D790
Tensile Impact Strength 710 kJ/m²
338 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
Exxon Method
Vicat Softening Point 65.0 °C
149 °F
1000g; ASTM D-1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746