ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
Exxon Method
Apparent Bulk Density 0.449 g/cc
0.0162 lb/in³
ASTM D1895 (B)
Viscosity 3100 cP

@Temperature 190 °C
3100 cP

@Temperature 374 °F
melt viscosity; ASTM D-3236
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
ASTM D2240
Tensile Strength, Ultimate 9.80 MPa
1420 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Modulus 0.00440 GPa
0.638 ksi
1% Secant, ASTM D790
Thermal Properties Metric English Comments
Melting Point 62.0 °C
144 °F
Exxon Method
Vicat Softening Point 76.0 °C
169 °F
Softening Point, R&B; ASTM E-28
Optical Properties Metric English Comments
Refractive Index 1.483
1.483
Exxon Method