ExxonMobil Escorene™ UL 00514 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 00514 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 00514 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 250°C (482°F) may cause resin degradation.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: CompoundingInjection MoldingFoamsWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ExxonMobil method
Vinyl Acetate Content 14 %
14 %
ExxonMobil method
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A
Tensile Modulus 0.0593 GPa
8.60 ksi
Molded Properties; ISO 527-2
Thermal Properties Metric English Comments
Melting Point <= 192 °C
<= 378 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 62.8 °C
145 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 250