Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 05540EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: Yes Applications: CompoundingHot Melt Adhesives Ink ModifierWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.967 g/cc
0.0349 lb/in³
ExxonMobil method
Vinyl Acetate Content 39 %
39 %
ExxonMobil method
Melt Flow 60 g/10 min
60 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
Molded Properties; ASTM D2240
Tensile Strength at Break >= 1.79 MPa
>= 260 psi
(20 in/min), Molded Properties; ASTM D638
Elongation at Break >= 750 %
>= 750 %
(20 in/min), Molded Properties; ASTM D638
Tensile Modulus 0.00303 GPa
0.440 ksi
(0.2 in/min), Molded Properties; ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 118 °C
<= 244 °F
Peak Melting Point; ExxonMobil method
Copyright © lookpolymers.com All Rights Reserved