ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:PP/TPO modification.EVA modification.Designed as a low density and high molecular weight polymer modifier to impart impact strength and toughness.Available as free flowing pellets.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaAll physical properties were measured from specimens cut from compression molded plaques per ASTM D 4703, Procedure A, Type I and conditioned at 23°C for a minimum of 40 hours per ASTM D 618 prior to testing. All stress/strain tests used specimens cut with a Type IV (Die C) die and tested with a grip separation of 25 mm (1") and a crosshead speed of 20 in./min.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.864 g/cc
0.864 g/cc
ASTM D1505
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 54

@Time 15.0 sec
54

@Time 0.00417 hour
0.12 in; ASTM D2240
Tensile Strength at Break 1.40 MPa
203 psi
ASTM D412 and ISO 37
Tensile Stress 1.40 MPa

@Strain 100 %
203 psi

@Strain 100 %
ASTM D412 and ISO 37
Elongation at Break 740 %
740 %
ASTM D412 and ISO 37
Flexural Modulus, 1% Secant 5.30 MPa
769 psi
ASTM D790 and ISO 178
Thermal Properties Metric English Comments
Heat of Fusion 44.0 J/g
18.9 BTU/lb
Crystallinity; ExxonMobil Method
Melting Point 41.0 °C
106 °F
Peak; ExxonMobil Method
Crystallization Temperature 26.0 °C
78.8 °F
ExxonMobil Method
Vicat Softening Point 42.0 °C
108 °F
ASTM D1525 and ISO 306/A
Glass Transition Temp, Tg -52.0 °C
-61.6 °F
ExxonMobil Method