Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for paintable automotive exterior applications.Availability: Europe Features:Balanced Stiffness/ToughnessDuctile High Impact ResistanceLow Temperature Impact ResistancePaintableUses: Automotive ApplicationsAutomotive BumperAutomotive Exterior PartsAutomotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 MPa
2000 psi
ISO 527-2/50
Tensile Strength, Yield 17.7 MPa
2570 psi
ISO 527-2/50
Elongation at Break 39 %
39 %
ISO 527-2/50
Elongation at Yield 3.5 %
3.5 %
ISO 527-2/50
Tensile Modulus 1.37 GPa
199 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.546 J/cm²

@Temperature -30.0 °C
2.60 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
0.693 J/cm²

@Temperature -20.0 °C
3.30 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ISO 75-2/A