ExxonMobil Exxtral™ BMU 141 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMU 141 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high scratch resistance and good UV resistance are required.Availability: Africa & Middle East and Europe Features:Balanced Stiffness/ToughnessGood Surface Finish High Impact ResistanceHigh Scratch ResistanceLow to No FoggingUses: Automotive ApplicationsAutomotive Instrument PanelAutomotive Interior PartsAutomotive Interior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Melt Flow 12 g/10 min
12 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527-2/50
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527-2/50
Elongation at Break 25 %
25 %
ISO 527-2/50
Elongation at Yield 3.2 %
3.2 %
ISO 527-2/50
Tensile Modulus 1.88 GPa
273 ksi
Secant; ISO 527-2
Flexural Strength 31.6 MPa
4580 psi
ISO 178
Flexural Modulus 1.86 GPa
270 ksi
ISO 178
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.714 J/cm²

@Temperature 0.000 °C
3.40 ft-lb/in²

@Temperature 32.0 °F
ISO 179
1.49 J/cm²

@Temperature 22.8 °C
7.10 ft-lb/in²

@Temperature 73.0 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.8 °C
208 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C
129 °F
ISO 75-2/A