Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, South America and North America Features: Good Creep ResistanceGood Dimensional StabilityGood Impact ResistanceGood Weather ResistanceHigh Stiffness Uses: Automotive ApplicationsAutomotive Exterior Parts Automotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.0 MPa
2030 psi
ISO 527-2/B
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527-2/B
Tensile Modulus 1.68 GPa
244 ksi
Secant; ISO 527-2
Flexural Modulus 1.89 GPa
274 ksi
ISO 178
Charpy Impact, Notched 0.441 J/cm²

@Temperature -30.0 °C
2.10 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.651 J/cm²

@Temperature -20.0 °C
3.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179
1.09 J/cm²

@Temperature 0.000 °C
5.20 ft-lb/in²

@Temperature 32.0 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2/A