Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMV 201 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMV 201 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive exterior parts including bumper fascia and rocker panels.Availability: North America Features: DuctileGood UV Resistance High FlowHigh Scratch ResistanceLow Temperature Impact ResistancePaintable Uses: Automotive ApplicationsAutomotive Bumper Automotive Exterior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183/A
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ISO 527-2
Flexural Modulus 1.69 GPa
245 ksi
0.079 in/min; ISO 178
Izod Impact, Notched (ISO) 39.9 kJ/m²
19.0 ft-lb/in²
ISO 180/A
Dart Drop, Total Energy 26.0 J

@Temperature -30.0 °C
19.2 ft-lb

@Temperature -22.0 °F
7.22 ft/sec; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 0.504 µm/m-°C

@Temperature -30.0 - 100 °C
0.280 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-2/Af
Copyright © lookpolymers.com All Rights Reserved