Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMV 208 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMV 208 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Polyolefin injection molding compound with very high flow, high stiffness, good low temperature impact resistance, and excellent processability for automotive exterior trim applications.Availability: North America Features: Good Impact ResistanceGood Processability High FlowHigh StiffnessLow Temperature Impact ResistancePaintable Uses: Automotive Exterior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183/A
Melt Flow 39 g/10 min

@Load 2.16 kg,
Temperature 230 °C
39 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527-2
Flexural Modulus 2.17 GPa
315 ksi
2.52 in, 0.079 in/min; ISO 178
Izod Impact, Notched (ISO) 27.3 kJ/m²
13.0 ft-lb/in²
ISO 180/A
Dart Drop, Total Energy 26.0 J

@Temperature -15.0 °C
19.2 ft-lb

@Temperature 5.00 °F
7.22 ft/sec; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-2/Af