ExxonMobil Exxtral™ BNT 013 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BNT 013 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessDuctileGood ColorabilityGood Surface Finish High Impact ResistanceLow Temperature Impact Resistance Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.0 MPa
2030 psi
ISO 527-2/50
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527-2/50
Elongation at Break 60 %
60 %
ISO 527-2/50
Elongation at Yield 4.0 %
4.0 %
ISO 527-2/50
Tensile Modulus 1.00 GPa
145 ksi
Secant; ISO 527-2/50
Flexural Modulus 0.951 GPa
138 ksi
Secant; ISO 178
Charpy Impact, Notched 0.861 J/cm²

@Temperature -30.0 °C
4.10 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
1.30 J/cm²

@Temperature 0.000 °C
6.20 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
2.52 J/cm²

@Temperature 22.8 °C
12.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 47.2 °C
117 °F
ISO 75-2/A