ExxonMobil Exxtral™ BNU 011 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BNU 011 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for injection molded automotive interior applications.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessDuctileGood ColorabilityGood Surface Finish High Impact ResistanceHigh Scratch Resistance Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.4 MPa
2380 psi
ISO 527-2/50
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 527-2/50
Elongation at Break 50 %
50 %
ISO 527-2/50
Elongation at Yield 4.0 %
4.0 %
ISO 527-2/50
Tensile Modulus 1.37 GPa
199 ksi
Secant; ISO 527-2/50
Charpy Impact, Notched 0.504 J/cm²

@Temperature -20.0 °C
2.40 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
0.735 J/cm²

@Temperature 0.000 °C
3.50 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
1.20 J/cm²

@Temperature 22.8 °C
5.70 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ISO 75-2/A