Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance are required.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/Toughness Good Dimensional StabilityGood ColorabilityGood Impact ResistanceGood Surface FinishLow to No Fogging Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.5 MPa
2540 psi
ISO 527-2/50
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527-2/50
Elongation at Break 21 %
21 %
ISO 527-2/50
Elongation at Yield 3.0 %
3.0 %
ISO 527-2/50
Tensile Modulus 2.10 GPa
305 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.315 J/cm²

@Temperature 0.000 °C
1.50 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
0.609 J/cm²

@Temperature 22.8 °C
2.90 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
ISO 75-2/A
Users viewing this material also viewed the following: