Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa & Middle East, Europe and North America Features: Good Impact ResistanceLow FlowUses: Automotive Applications Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.15 GPa
167 ksi
ISO 527-2
Flexural Strength 31.0 MPa
4500 psi
ISO 178
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched (ISO) 27.3 kJ/m²
13.0 ft-lb/in²
Partial Break; ISO 180
Charpy Impact, Notched 0.294 J/cm²

@Temperature -20.0 °C
1.40 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
0.399 J/cm²

@Temperature 0.000 °C
1.90 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
2.52 J/cm²

@Temperature 22.8 °C
12.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.1 °C
169 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C
118 °F
ISO 75-2/A