Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessGood Impact ResistanceGood UV ResistanceLow EmissionsLow to No FoggingLow to No Odor Uses: Automotive ApplicationsAutomotive Exterior PartsAutomotive Exterior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ISO 1183
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527-2/50
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2/50
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/50
Elongation at Yield 5.5 %
5.5 %
ISO 527-2/50
Tensile Modulus 1.10 GPa
160 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.504 J/cm²

@Temperature -20.0 °C
2.40 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
0.672 J/cm²

@Temperature -5.00 °C
3.20 ft-lb/in²

@Temperature 23.0 °F
Complete Break; ISO 179
1.09 J/cm²

@Temperature 22.8 °C
5.20 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C
172 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C
118 °F
ISO 75-2/A